TExcelTAD
Home › Analog Electronics: Diodes, Transistors & Op-Amps › Semiconductors for Circuit Designers: Bands, Carriers and Doping

Semiconductors for Circuit Designers: Bands, Carriers and Doping

Why does a diode's leakage current double every few kelvin? Why is a silicon diode's drop about 0.6 V0.6\ \text{V} but a red LED's about 1.8 V1.8\ \text{V}? Why does a transistor amplifier that works on the bench drift when the board warms up? Each answer comes from a handful of facts about semiconductors: the band gap, the two kinds of carrier, doping and temperature. This lesson gives just those facts, at the level a circuit designer needs to read a datasheet and trust a device model. The full device physics (band diagrams of junctions, transport equations, fabrication) is the subject of the planned chip-design courses of the Embedded Systems & Chip Design track.

Bands and the band gap

In a single atom, electrons sit at sharp energy levels. In a crystal of 5×10225 \times 10^{22} atoms per cm3\text{cm}^3 the levels of neighbouring atoms overlap and spread into bands. Two bands matter:

  • the valence band, full of the electrons that form the covalent bonds;
  • the conduction band, the next band up, where an electron is free to move through the crystal.

Between them lies the band gap EgE_g, an energy range with no allowed states. Whether a material conducts depends on the gap:

Material EgE_g at 300 K Typical use
metal (copper) none (bands overlap) conductors
germanium 0.66 eV0.66\ \text{eV} early transistors, IR detectors
silicon 1.12 eV1.12\ \text{eV} almost all diodes, transistors and ICs
gallium arsenide 1.42 eV1.42\ \text{eV} RF transistors, IR LEDs
silicon carbide (4H) 3.26 eV3.26\ \text{eV} high-voltage power devices
gallium nitride 3.4 eV3.4\ \text{eV} blue LEDs, fast power transistors
glass, ceramics >5 eV> 5\ \text{eV} insulators

A semiconductor's gap is small enough that heat lifts a few electrons across it at room temperature. The gap also sets the photon energy of an LED (E=hc/λE = hc/\lambda, so a wider gap gives bluer light, LEDs and Photodiodes) and, roughly, how much voltage a junction drops when it conducts.

intrinsic n-type (donors) p-type (acceptors) conduction band valence band EC EV EF Eg = 1.12 eV ED EF EA EF electron hole

Two carriers: electrons and holes

When an electron leaves a bond for the conduction band it leaves behind a missing bond, a hole. A neighbouring bonded electron can hop into the hole, so the hole moves; it behaves exactly like a positive carrier of charge +q+q. A pure (intrinsic) semiconductor therefore has equal numbers of free electrons and holes, n=p=nin = p = n_i. For silicon at 300 K300\ \text{K} this course uses

ni≈1.0×1010 cm−3n_i \approx 1.0 \times 10^{10}\ \text{cm}^{-3}

(published values range from about 1.01.0 to 1.5×10101.5 \times 10^{10}; modern references give 9.65×1099.65 \times 10^9). That is one free electron per 5×10125 \times 10^{12} atoms: intrinsic silicon is a poor conductor.

The intrinsic density grows steeply with temperature, because the thermal energy kTkT (25.85 meV25.85\ \text{meV} at 300 K) must supply a gap of 1.12 eV1.12\ \text{eV}:

ni(T)∝T3/2exp⁡(−Eg2kT)n_i(T) \propto T^{3/2} \exp\left(-\frac{E_g}{2kT}\right)

This one exponential explains why every leakage current in silicon rises fast with temperature.

Doping

Replace a few silicon atoms (group IV) by phosphorus or arsenic (group V, donors). Each donor has one electron more than the bonds need, held so weakly (its level EDE_D is about 0.045 eV0.045\ \text{eV} below the conduction band) that at room temperature practically every donor gives its electron away. The result is n-type silicon, with electrons as majority carriers. Boron (group III, an acceptor) has one electron too few; it captures a bonded electron and creates a hole: p-type silicon, with holes as majority carriers. The dopant ions left behind are fixed charges; they cannot move.

In equilibrium the product of the two densities is fixed by the material and temperature, whatever the doping (the mass-action law), and the crystal stays neutral:

n p=ni2,n+NA=p+NDn\,p = n_i^2, \qquad n + N_A = p + N_D

For n-type silicon with ND≫niN_D \gg n_i this gives n≈NDn \approx N_D and the minority density p≈ni2/NDp \approx n_i^2/N_D, tiny but important: minority carriers are what cross a forward-biased junction and what makes up a diode's reverse leakage (The PN Junction).

Drift, diffusion and conductivity

Carriers move in two ways. Drift: an electric field pushes them, with an average velocity v=μEv = \mu E set by the mobility μ\mu; electrons in lightly doped silicon have μn≈1350 cm2/(V⋅s)\mu_n \approx 1350\ \text{cm}^2/(\text{V} \cdot \text{s}), holes μp≈480 cm2/(V⋅s)\mu_p \approx 480\ \text{cm}^2/(\text{V} \cdot \text{s}). That gives a conductivity

σ=q (nμn+pμp),ρ=1σ\sigma = q\,(n\mu_n + p\mu_p), \qquad \rho = \frac{1}{\sigma}

Diffusion: where the carrier density changes from place to place, random thermal motion carries more of them from the crowded side to the sparse side, with no field needed. Diffusion is what drives current across a forward-biased PN junction and through the base of a bipolar transistor. Electrons are about three times as mobile as holes, which is why n-channel MOSFETs and NPN transistors are preferred where speed matters.

Worked example

Given: silicon at 300 K300\ \text{K} doped with ND=1016 cm−3N_D = 10^{16}\ \text{cm}^{-3} phosphorus; ni=1.0×1010 cm−3n_i = 1.0 \times 10^{10}\ \text{cm}^{-3}, μn=1350\mu_n = 1350, μp=480 cm2/(V⋅s)\mu_p = 480\ \text{cm}^2/(\text{V} \cdot \text{s}).

Find: nn, pp, the resistivity, and how it compares with intrinsic silicon.

Solve:

n≈ND=1.0×1016 cm−3,p=ni2n=10201016=1.0×104 cm−3ρ=1qnμn=11.602×10−19 C⋅1016 cm−3⋅1350 cm2/(V⋅s)=0.462 Ω⋅cmρi=1qni(μn+μp)=3.41×105 Ω⋅cm\begin{aligned} n &\approx N_D = 1.0 \times 10^{16}\ \text{cm}^{-3}, \qquad p = \frac{n_i^2}{n} = \frac{10^{20}}{10^{16}} = 1.0 \times 10^{4}\ \text{cm}^{-3} \\ \rho &= \frac{1}{q n \mu_n} = \frac{1}{1.602 \times 10^{-19}\ \text{C} \cdot 10^{16}\ \text{cm}^{-3} \cdot 1350\ \text{cm}^2/(\text{V} \cdot \text{s})} = 0.462\ \Omega \cdot \text{cm} \\ \rho_i &= \frac{1}{q n_i (\mu_n + \mu_p)} = 3.41 \times 10^{5}\ \Omega \cdot \text{cm} \end{aligned}

Check: one donor per five million atoms lowers the resistivity by a factor of about 7×1057 \times 10^5, and the holes (104 cm−310^4\ \text{cm}^{-3}) contribute nothing measurable to the conduction. A 0.46 Ω⋅cm0.46\ \Omega \cdot \text{cm} wafer is a typical starting material for devices.

In Python

The same numbers, plus nin_i at other temperatures. The model keeps EgE_g fixed at 1.12 eV1.12\ \text{eV}, a simplification (the real gap shrinks slightly as silicon warms, so the true nin_i at 400 K is somewhat higher).

python · try it yourself
import numpy as np

q, k = 1.602e-19, 8.617e-5          # C, eV/K
EG, NI300 = 1.12, 1.0e10            # eV, cm^-3 (silicon, 300 K)
MU_N, MU_P = 1350, 480              # cm^2/(V s), lightly doped silicon

def ni(T):
    return NI300 * (T / 300)**1.5 * np.exp(-EG / (2 * k) * (1 / T - 1 / 300))

for T in [250, 300, 350, 400]:
    print(f"T = {T} K: n_i = {ni(T):.3e} cm^-3")

ND = 1e16                           # donors, cm^-3
n = ND / 2 + np.sqrt((ND / 2)**2 + NI300**2)
p = NI300**2 / n
rho = 1 / (q * (n * MU_N + p * MU_P))
rho_i = 1 / (q * NI300 * (MU_N + MU_P))
print(f"n-type 1e16: n = {n:.3e}, p = {p:.3e} cm^-3")
print(f"resistivity: doped {rho:.3f} Ohm cm, intrinsic {rho_i:.3e} Ohm cm")
T = 250 K: n_i = 9.992e+07 cm^-3
T = 300 K: n_i = 1.000e+10 cm^-3
T = 350 K: n_i = 2.782e+11 cm^-3
T = 400 K: n_i = 3.463e+12 cm^-3
n-type 1e16: n = 1.000e+16, p = 1.000e+04 cm^-3
resistivity: doped 0.462 Ohm cm, intrinsic 3.411e+05 Ohm cm

From 300 to 350 K, nin_i grows 28 times. A device's leakage current is proportional to ni2n_i^2 and so grows about 770 times over the same 50 K. This is the root of the "leakage doubles every few kelvin" rule and of the bias drift studied in Bias Stability. At a few hundred kelvin above room temperature nin_i would reach the doping level and the device would stop behaving as doped silicon; wide-gap materials (SiC, GaN) push that limit far higher, one reason they suit hot power electronics.

Guided lab: light makes carriers

Hand calculation. A photon with more energy than EgE_g lifts an electron across the gap, creating an electron-hole pair, so a semiconductor's conductivity rises with light. A cadmium sulphide light-dependent resistor (LDR, Eg≈2.4 eVE_g \approx 2.4\ \text{eV}) responds to visible light.

Simulation. The Python model above for the temperature effect; light acts the same way, adding carriers.

What you would measure. Measure an LDR with a multimeter on its resistance range: typically around 1 MΩ1\ \text{M}\Omega in a closed hand, a few kΩ\text{k}\Omega under a desk lamp and a few hundred ohms in sunlight (datasheet ranges vary by a factor of 2 to 3 between parts). Then put it in a divider with 10 kΩ10\ \text{k}\Omega from a 5 V5\ \text{V} supply and watch the divider voltage swing from near 00 to over 4 V4\ \text{V}. Expect the reading to lag a sudden change by tens of milliseconds: CdS cells are slow, unlike the photodiodes later in the course.

Hazards and safe setup. Low voltage only. CdS cells contain cadmium: don't break or burn them, and dispose of them as electronic waste (cadmium is a restricted substance under the EU RoHS directive 2011/65/EU; the narrow exemption for CdS photoresistors in professional-audio optocouplers was set to expire at the end of 2013, so equipment for the EU market has largely moved to photodiodes and phototransistors, though the parts are still sold as components).

Pitfalls

  • Holes are not positrons. A hole is a missing bond electron; it moves because bonded electrons move the other way.
  • Doping does not charge the crystal. Each donor electron leaves a positive ion behind; n-type silicon is neutral.
  • "Minority" does not mean "negligible". Minority carriers set diode leakage, the Shockley law and the bipolar transistor's action.

Practice

  1. P-type silicon has NA=5×1017 cm−3N_A = 5 \times 10^{17}\ \text{cm}^{-3}. Find pp and nn at 300 K.
  2. Using ni2n_i^2, by what factor does a diode's leakage change between 300 K and 250 K in the model above?
  3. Why is GaN used for blue LEDs, while silicon is not used for LEDs at all?
Answer
  1. p≈5×1017 cm−3p \approx 5 \times 10^{17}\ \text{cm}^{-3}, n=1020/(5×1017)=200 cm−3n = 10^{20}/(5 \times 10^{17}) = 200\ \text{cm}^{-3}.
  2. (9.99×107/1010)2≈1.0×10−4(9.99 \times 10^7 / 10^{10})^2 \approx 1.0 \times 10^{-4}: leakage is about 10 000 times smaller at 250 K.
  3. Blue photons carry about 2.7 eV2.7\ \text{eV}, which needs a gap at least that wide; GaN has 3.4 eV3.4\ \text{eV} (alloyed with indium to tune the colour). Silicon's gap is 1.12 eV1.12\ \text{eV} (infrared) and indirect, so it emits light very inefficiently.

Test yourself

Doping silicon with phosphorus (group V) produces…

  1. p-type silicon, holes in the majority
  2. n-type silicon, electrons in the majority
  3. intrinsic silicon
  4. a negatively charged crystal

N-type silicon has n=1016 cm−3n = 10^{16}\ \text{cm}^{-3} and ni=1010 cm−3n_i = 10^{10}\ \text{cm}^{-3}. The hole density is…

  1. 1016 cm−310^{16}\ \text{cm}^{-3}
  2. 1010 cm−310^{10}\ \text{cm}^{-3}
  3. 104 cm−310^{4}\ \text{cm}^{-3}
  4. 106 cm−310^{6}\ \text{cm}^{-3}

Why does a silicon device's leakage current rise steeply with temperature?

  1. the doping level rises
  2. nin_i grows like T3/2e−Eg/2kTT^{3/2} e^{-E_g/2kT}, and leakage scales with ni2n_i^2
  3. the band gap doubles
  4. mobility increases

Which carrier type has the higher mobility in silicon?

  1. holes
  2. electrons
  3. they are equal
  4. dopant ions